According to the working environment of the glass tank furnace, considering various factors cause the kiln lining damage: chemical erosion and mechanical erosion, degree of volatility and high temperature, such as the choice of kiln material basically has the following series:
(1) AI203 - Si02 series; Mainly includes the clay brick and silicon brick.
(2) AI2O3 Zr02 - Si02 series; Mainly include zircon brick and zirconium fused corundum brick.
(3) Zr02 - Sio2 series;
(4) the MgO style - AI203, MgO style - Cr203, MgO style - Sioz series;
(5) heat insulation material